Conventional Interconnect PV Ribbon Machine
Brand:CRM
Generally, conventional interconnect PV ribbon wire machines are used for producing solar panel ribbons, essential components. In addition to connecting solar cells within a module, these machines create flat, tinned copper conductors that transmit electrical energy efficiently. With the help of advanced multi-cage rolling mills, copper wires are rolled and flattened to precise dimensions. Moreover, the machine incorporates annealing, which softens the copper, and tinning, which enhances corrosion resistance and solderability. In addition to providing high output and efficiency, these interconnect PV ribbon and wire machines are capable of producing at speeds ranging from 100 to 300 meters per minute. Servo winding and cooling mechanisms ensure consistency of quality throughout the production process through precision control systems. High-quality PV ribbons result from this advanced Conventional Interconnect PV Ribbon Machine technology, which make solar panels more durable, efficient, and perform better. Sky Bluer Environmental Technology Co., Ltd made a huge update in annealing method in 2024, developing the traditional short-circuit annealing into a safer induction annealing for the Interconnect PV Ribbon Machine.
Yes, In the table below you will find all the sizes produced by our Interconnect PV Ribbon Wire Machine
# | PV Ribbon Products | Parameter | Industry Standard | Other Company | CRM |
1 |
Conventional Interconnect PV Ribbon | Coating thickness | ±5μm | 25±5μm | 25±3μm |
Finished product thickness | ≥0.01mm | ≥0.015mm | ≥0.01mm | ||
Finished product width | ±0.05mm | ±0.05mm | ±0.05mm | ||
Tensile strength | ≥110Mpa | ≥150Mpa | ≥170Mpa | ||
Elongation | ≥15% | ≥25% | ≥25% | ||
Yield strength | ≤70Mpa | ≤70Mpa | 62.68Mpa | ||
Sickle bend | ≤5mm/m | ≤4mm/m | ≤4mm/m | ||
Resistivity | 0.30Ω* mm²/m | 0.02-0.023Ω* mm²/m | 0.0230 Ω* mm²/m | ||
Aging resistance | - | - | DH2000 | ||
Corrosion resistance | Salt spray test | Salt spray test 48h | Salt spray test 48h | ||
2 |
Conventional Interconnect PV BusBar | Coating thickness | ±5μm | 25±5μm | 25±3μm |
Finished product thickness | ≥0.01mm | ±0.015mm | ±0.015mm | ||
Finished product width | ±0.05mm | ±0.05mm | ±0.05mm | ||
Tensile strength | ≥120Mpa | ≥150Mpa | ≥170Mpa | ||
Elongation | ≥18% | ≥25% | ≥25% | ||
Sickle bend | ≤5mm/m | ≤3mm/m | ≤3mm/m | ||
Resistivity | 0.30Ω* mm²/m | 0.02-0.023Ω* mm²/m | 0.0230 Ω* mm²/m | ||
Aging resistance | - | - | DH2000 | ||
Corrosion resistance | Salt spray test | - | Salt spray test 48h | ||
3 |
Multi-Busbar (MBB) PV Ribbon | Diameter | - | -0.003+0.012mm | -0.005,+0.015mm |
Average coating thickness | ±5μm | 17±4μm | 17±3μm | ||
Yield strength | ≤70Mpa | ≤70Mpa | ≤62.68Mpa | ||
Elongation | ≥15% | ≥25% | ≥25% | ||
Resistivity | 0.30Ω* mm²/m | ≤0.025Ω* mm²/m | ≤0.021Ω* mm²/m |
What Photovoltaic Ribbon and BusBarEquipment Can We Manufacture?
Photovoltaic Busbar Production Line
MBB Double Wire PV Ribbon Machine
PV Ribbon Machine With Tin Coating Lines
Photovoltaic Bus Bar Rolling Machine With Tin Coating Lines
PV Ribbon Machine With Tin Coating Lines
Copper Wire And Photovoltaic Ribbon Machine
Contact Us Today
Email: [email protected]
Mobile/ Whatsapp:+86 13861313954
Website: https://precision-rolls.com/Products/